A210 Seamless Boiler Steel Tube

A210 Seamless Boiler Steel Tube

Seamless medium-carbon steel boiler and super heater tubes.
● Application: for boilers, super heaters, steam line pipes of boiler
● Size range: O.D.: 12.7-114.3mm W.T.: 1.65-10mm L.: 18000mm max

질문이 있으시면,문의하시기 바랍니다:sales@grandsteeltube.com

  • 묘사
  • Baosheng의 장점
  • 사양
  • 문의

ASTM A210 is the standard covers seamless medium-carbon steel boiler and superheater tubes. ASTM A210 also covers minimum-wall-thickness, tubing sizes, boiler flues including safe ends, arch and stay tubes. ASTM A210 provides tensile and hardness properties but only applicable to certain size limitations. Material manufacturing shall be killed. Tubes shall be made by seamless process, marked as either hot-finished or cold-finished. Surface condition shall be specifically stated in the order. Chemical composition shall conform to the requirements. Elemental composition other than listed here shall not be permitted. Tension test, flattening test, flaring test, hardness test, hydrostatic or nondestructive electric test shall be made on specimens. Superheater tubes shall be formed without defects and shall withstand expansion, 구슬로 장식, forging, welding, and bending.

ASTM A210 seamless medium carbon steel pipe is applied for boiler pipe and boiler flue pipe with the minimum thickness, including safety end, vault, supporting pipe and super heater pipe.

질문이 있으시면,당신은 연락을 환영합니다 sales@grandsteeltube.com

1. Production of A210 seamless steel tubes since 2005.

2. 유럽 고객과 협력,북아메리카,남아메리카,이후 등 2006.

3. 샘플은 이내에 배송 될 수 있습니다. 25 확인 후 일

4. 40 생산 기간으로 일 및 주문 확인 후 배송.

5. 15,000 meters of seamless steel tubes in stock.

6. 200 크기는 OD에서 제안될 수 있습니다:12.7mmxWT:1.65밀리미터 내지 외경:114.3mmxWT:10밀리미터

7. 다음과 같은 제3자 검사:투브,증권 시세 표시기,증권 시세 표시기,기타 허용

8. 전문 팀은 귀하의 특수 튜브 요구 사항을 지원합니다..

9. 다른 관련 튜브:A179,A192,A213 seamless steel tube;등

질문이 있으시면,당신은 연락을 환영합니다 sales@grandsteeltube.com

Table 1: Steel grade and chemical composition:

C 미네소타 P S Si
A-1 ≤0.27 ≤0.93 ≤0.035 ≤0.035 ≥0.10
C ≤0.35 0.29-1.06 ≤0.035 ≤0.035 ≥0.10

Table 2: Mechanical property:

Tensile Strength Mpa/ksi Yield Point (Mpa/ksi) 신장 %
A-1 ≥255/37 ≥415/60 ≥30
C ≥275/40 ≥485/70 ≥30

Table 3: Tolerance for O.D. and W.T.(SA-450/SA-450M)

외경. inch (밀리미터) + - W.T. inch (밀리미터) + -
<1(25.4) 0.10 0.10 ≤1.1/2”(38.1) 20% 0
1”-1.1/2”(25.4-38.1) 0.15 0.15 >1.1/2(38.1) 22% 0
1.1/2”-2”(38.1-50.8) 0.20 0.20 - - -
2”-2.1/2”(50.8-63.5) 0.25 0.25 - - -
2.1/2”-3”(63.5-76.2) 0.30 0.30 - - -
3”-4”(76.2-101.6) 0.38 0.38 -

접촉 우리